It is constructed from Portland gypsum cement and sand using either precast or cast in situ technique. For precast production technique, the casted artificial marble will be stripped from the mould after three days and then treated with liquid fluorite of magnesia solution at the age of five days. After that, the stone is washed and wrapped with paper for 24 hours and treated again with the same solution, and it will be polished at the final stage at the age of 30days. For in situ construction method, layer of prepared mixture is placed on a canvas, and the thickness of the layer shall be 1.5 mm greater than the required thickness of the stone to be constructed. The surface of the laid layer is rubbed and then polished properly.